GettyImages-1258166774.jpg

Ultrasonic Thickness Testing

GettyImages-1258166774.jpg

This course covers essential concepts in ultrasonic thickness testing, including sound properties, equipment setup, wave modes, calibration, and signal interpretation. It supports foundational knowledge for technicians working with UT thickness measurements.

This lesson also demonstrates how to calibrate UT Thickness instruments including Digital and A-scan, take actual measurements, and collect/document results. It is ideal for those individuals who will be taking thickness measurements with UT instruments and/or are pursuing Limited Level II UT Thickness certification. It is also applicable for those who will be providing oversight on UT Thickness operations.

GettyImages-1258166774.jpg

Course Overview

This course addresses the required training by documents controlling the certification program, such as NAS-410, SNT-TC-1A, and NavSea Technical Publication T9074-AS-GIB-010/271. This course content conforms to the training subjects listed in ANSI/ASNT CP-105, Standard Topical Outlines for Qualification of Nondestructive Testing Personnel. It is intended that the course shall include the online training as well as laboratory-type hands-on training under the direction of a level II or level III to meet the total hours of training required by the applicable certification document listed above.

Upon Completion, Learners Will Have Covered:

  • Ultrasonic sound and particle displacement; particle density and elasticity as it affects the velocity of sound, cycles, wavelength, frequency, and hertz
  • Piezoelectric crystals, transducer parts, generating ultrasound, pulse echo, and continuous sound transmission; equipment controls
  • Velocity as it relates to thickness determination, acoustic impedance, interface definition, ultrasonic wave modes and properties, mode conversion, refracted angles, Snell’s Law
  • Couplant; surface effects on sound transmission; sound reflection; near field and far field definition; attenuation definition
  • “A”, “B”, and “C” scan presentations; digital readout and “A” scan ultrasonic thickness testing units; painted surface testing
  • Transducer capabilities, efficiencies, different types of transducers for testing, pitch catch transducer, and connectors for transducers
  • Calibration standard types and materials; selection of equipment and transducers
  • Signal display attributes for “A” scan presentations: broadband and narrowband waveforms
  • Testing variables such as surface condition, doubling, gating, discontinuities, temperatures, records, and types of couplants
  • Qualification and certification documents, and a review of SNT-TC-1A

This course meets the recommendations for training as described in SNT-TC-1A.

NOTE: The completion of these assignments in addition to self-study is strongly encouraged and will add to the overall training benefit and time to be credited. It will also better prepare the student for the practical lab/hands-on session. It is recommended that the student a log of the self-study time. It is also recommended that the applicable Level III be involved and confirm that the reading and self-study assignments have been completed. This should become a part of the student's training records which may be used in conjunction with subsequent certifications.

 

At a Glance

L_Money_Bill_Cash.svg

Price

$825
L_Open Book.svg

Access to Course Materials

60 days

L_Clock.svg

Course Length & Earnings

Approximately 14 hours

Course Details

  • Benefits
  • Course Modules
  • COMPREHENSIVE
    Meets all ASNT ANSI SNT-TC-1A recommendations per CP-105. Students can typically retain 25% to 60% more of the information as compared to traditional classroom training.
  • EASY TO ACCESS
    Participants can access the course 24/7 from any computer running Google Chrome browser with an internet connection.
  • EASY TO USE
    Pause to take notes with ability to retake lesson quizzes as needed. Online learning gives the student complete control over their learning experience.
  • EASY TO UNDERSTAND
    Audio/Video narration, demonstrations, animated graphics and video footage make even the most complex topics engaging and easy-to-understand.
  • PROVEN METHODS
    Detailed video demonstrations, practice problems, and quizzes facilitate the mastery of concepts and measure content retention.
  • RELIABLE
    Course content was developed by Chuck Hellier with industry experts and NDT Classroom Inc. learning professional Kevin Crosby, Phd in curriculum design.
  • ACCESS TO NDT CLASSROOM INSTRUCTOR
    Users can contact NDT Classroom instructors by emailing info@NDTclassroom.com or calling 716-262-8870.
  • LIVE SUPPORT
    NDT Classroom customer support Monday through Friday 8:30 AM to 5:00 PM EST. at info@NDTclassroom.com or 716-262-8870
  • Chapter 1 – General Ultrasonic Theory
  • Chapter 2 – Equipment
  • Chapter 3 – Sound Properties and Wave Modes
  • Chapter 4 – Sound Travel, Couplant, Material Structure
  • Chapter 5 – Screen Presentation and Equipment Types
  • Chapter 6 – Transducers and Properties
  • Chapter 7 – Reference Standards, Calibration and Settings
  • Chapter 8 – Waveforms
  • Chapter 9 – Test Performance Variables
  • Chapter 10 – Qualification and Certification Requirements
  • Chapter 11 – Equipment Demo
  • Final Exam

Meet the Instructor


  • Gary Larson

    Gary Larson

    Gary Larson brings over 40 years of NDT experience across industries including nuclear, aerospace, and manufacturing. He holds ASNT Level III certifications in RT, UT, PT, MT, and VT, along with ACCP credentials. Gary has worked with Sikorsky and Pratt & Whitney, providing inspection and training in multiple methods. He currently consults as a Level III for aerospace and military suppliers and contributes to ASTM’s E07 Committee. His teaching experience includes developing and delivering online NDT courses.

Frequently Asked Questions

  • How much do I need to know before taking this course?

    You don’t need to have any background in NDT to take this course. It will prepare you to take the practical training needed to become certified by your employer.

  • Who should take this course?

    Anyone interested in expanding their welding career to examine welds and other types of materials and products.

  • How long do I have to complete this course?

    You have 30 days to take the course and 10 days to complete the exam.

  • Does this course include a completion exam?

    Yes, you will not only take quizzes after many of the chapters, there is a final exam after the successfully complete the course.

  • Do I need to purchase any other materials?

    We recommend you use the ASNT classroom Guide Book Item Number: 1642.

  • Does the time I spend in this course count towards the recommended number of training hours per ASNT SNT-TC-1A?

    Yes, all of the time you spend in the course, any reading time and hands on practical training all count towards the recommended number of training hours.

  • Can I use these hours for recertification?

    Yes, you can use this time towards your recertification.

  • What platforms and devices can I use to view the courses?

    You must be connected to the internet to access our online courses. We support the most recent versions of Google Chrome, Firefox, Safari, and Internet Explorer. Courses can be viewed on desktops, laptops, tablets, and mobile phones. Note, however, that a high speed internet connection and large screen offer a better user experience.

Comprehensive support for your welding education journey

Customer support representative assisting a client

Comprehensive support for your welding education journey

Customer support representative assisting a client
Questions about course content?
Running into a technical issue?


Our dedicated support team is here to make sure your welding education experience stays on track. Visit our Learning Support page, select the type of help you need from the dropdown menu, and a team member will be in touch promptly.
Customer support representative assisting a client