25 Hardfacing Tips: A Best Weld Overlay Practice
Maximize the benefits of your hardfacing applications
October 2024
Hardfacing improves the service life and efficiency of metal parts that are subject to wear. Simply choosing the right product will not guarantee a good result. The base metal, wear mechanism, welding process, and application details are all equally important factors. Here are 25 guidelines that will assist in maximizing the benefits of your hardfacing applications.
Base Metal Considerations
1. Identify the base metal along with its carbon and alloy contents. Common base metals include carbon st..