Lasers: The Best Fit(up) for Welding?
For many manufacturers, the laser has become the default tool for easier welding
May 2024
For many (or most) manufacturers, the laser has become the default tool for creating sheet metal blanks. The advantages are as obvious as they are plentiful: high throughput, flexible geometry, high accuracy, low operating costs, no tooling requirement, and so on. The downstream effects are also a bonus. While a waterjet proves an ideal edge condition, it is slow and expensive to run. A punch or turret can achieve high throughput and offer the additional benefit of enabling forming operations, but witness marks may..