Renewed Opportunities for Girth Welding in High-Strength Pipelines

Self-shielded flux cored arc welding has become a viable option for pipeline operators
March 2023
By: RADHIKA R. PANDAY 

Self-shielded flux cored arc welding (FCAW-S) was invented in 1959 as an alternative to shielded metal arc welding (SMAW) to improve productivity and reduce cost. It was introduced as a semiautomatic tubular wire process with conventional equipment: a constant-voltage, direct current power supply; a wire welding gun; and a wire feeder. As shown in Fig. 1, the key difference between FCAW-S and other open-arc welding processes is the absence of shielding gas. FCAW-S employs an arc in air without the intended shieldin..

Join AWS to read the full article

Get access to key insights and premium industry news today!
Already a member? Log In

D_Magnifying_Glass_Search.svg

Search Articles 

Find past articles by date, topic, or keyword.
D_PDF.svg

Publication Archive

View past issues of our magazines, including Welding Journal Research Supplement in PDF format.

D_Globe.svg

AWS News

Stay up to date on the latest announcements from AWS.