As more energy infrastructure is needed to keep the world going, important technologies and techniques in the field of underwater welding have moved to the forefront. Due to the application versatility of underwater welding, the welding industry is consistently looking for innovative ways to use this process to help clients stay on schedule and reduce costs.
Phoenix Achieves Permanent Underwater Welding
For 2..